C68410
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | B | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||||||||
| Min (%) | 59.0 | .03 | .001 | .20 | 1.0 | ||||||
| Max (%) | 64.0 | .09 | .50 | Rem | 1.0 | .30 | .50 | .50 | .03 | 1.5 | 1.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Bar | As Hot Extruded | M30 |
60.9 Min 69.6 Typ 81.2 Max |
12 Min 35 Max |
110 Min 155 Max |
| Forgings | As Hot Forged - Air Cooled | M10 |
65.2 Min 75.4 Typ 87.0 Max |
12 Min 40 Max |
115 Min 165 Max |
| Melting Point - Solidus°F | 1512 |
|---|---|
| Densitylb/cu in. at 68°F | 0.28 |
| Electrical Conductivity% IACS at 68°F | 87.1 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 38.2 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.098 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Fittings and valves | ||
| Valve Bodies, Faucets and Plumbing Componsnts |
Applicable Specifications
Corrosion Properties