C69050
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Zn | Ni(3) | Al | Si | Zr | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||
| Min (%) | 70.0 | 0.50 | 3.0 | 0.10 | 0.01 | |
| Max (%) | 75.0 | Rem | 1.5 | 4.0 | 0.6 | 0.20 |