Find suppliers for this alloyC69100
Chemical Composition
Element
Cu(1)PbSnZnFeNiAlMnSi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)81.00.80.70.8
Max (%)84.00.050.10Rem0.251.41.20.101.3
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Rockwell B scale
Shear Strength
(ksi)
Section Size
(in)
TubeCast and Annealed (homogenized)O1070   Typ
35   Typ
45   Typ
72   Typ
37   Typ
0.022
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F2012
Melting Point - Solidus°F1846
Densitylb/cu in. at 68°F0.308
Specific Gravity8.53
Electrical Conductivity% IACS at 68°F15
Coefficient of Thermal Expansion 68-21210⁻⁶ per °F (68 – 212°F)10.6
Coefficient of Thermal Expansion 68-39210⁻⁶ per °F (68 – 392°F)10.6
Modulus of Elasticity in Tensionksi16900
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldNot Recommended
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedNot Recommended
Forgeability Rating55
Machinability Rating78
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialTube, hydraulic and pneumaticForming CharacteristicsFormability
Tube, hydraulic and pneumaticMagnetic PropertiesNon-Magnetic
Tube, hydraulic and pneumaticMechanical PropertiesCryogenic Properties
Tube, hydraulic and pneumaticSolderabilitySolderability
Applicable Specifications
Form Sub-Form System Standard Description
PipeASTMB706SEAMLESS COPPER ALLOY (UNS NO. C69100) PIPE AND TUBE
Seamless Pipe and TubeC69100 AlloyASMESB706SEAMLESS PIPE AND TUBE
TubeASTMB706SEAMLESS COPPER ALLOY (UNS NO. C69100) PIPE AND TUBE
Corrosion Properties

No information available.