Find suppliers for this alloy
C69220
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Mn | Sb | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||||||
| Min (%) | 69.0 | 0.05 | 0.8 | 1.8 | ||||||
| Max (%) | 71.0 | 0.08 | 0.30 | Rem | 0.10 | 0.20 | 0.20 | 1.8 | 0.10 | 2.6 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | 1/4 Hard | H01 |
82 Min 84 Typ 85 Max |
46 Min 48 Typ |
140 Min |
|
| Rod | 1/4 Hard | H01 |
82 Min 84 Typ 85 Max |
46 Min 48 Typ |
30 Min |
140 Min |
| Melting Point - Liquidus°F | 1598 |
|---|---|
| Melting Point - Solidus°F | 1592 |
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.3 |
| Electrical Conductivity% IACS at 68°F | 9.5 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 18.02 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.34 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 10.34 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 0 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.089 |
| Modulus of Elasticity in Tensionksi | 14900 |
| Modulus of Rigidityksi | 6092 |
| Poisson's Ratio | 0.32 |
| Technique | Suitability |
|---|---|
| Forgeability Rating | 95 |
| Machinability Rating | 78 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 968 | |||
| Hot Working Temperature | 1148 | |||
| Precipitation Treatment | 932 | |||
| Solution Treatment | 1436 | |||
| Stress Relief | 770 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Automotive Parts | ||
| Electrical | Electronic parts | ||
| Plumbing | Drinking water Fixtures, Plumbing |
Applicable Specifications
Corrosion Properties