Find suppliers for this alloy
C69240
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||||||
| Min (%) | 71.0 | 0.06 | 0.10 | 0.6 | 1.8 | ||||
| Max (%) | 72.5 | 0.25 | 0.30 | Rem | 0.20 | 0.12 | 0.50 | 1.2 | 2.2 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Bar | 1/2 Hard | H02 |
83.0 Typ |
50.0 Typ |
25 Typ |
70 Typ |
| 1/2 Hard and Stress Relieved | HR02 |
75.0 Typ |
54.0 Typ |
29 Typ |
70 Typ |
|
| Extruded and Drawn | H50 |
83.0 Typ |
46.0 Typ |
21 Typ |
70 Typ |
|
| Rod | 1/2 Hard | H02 |
77.0 Typ |
45.0 Typ |
21 Typ |
90 Typ |
| Melting Point - Liquidus°F | 1610 |
|---|---|
| Melting Point - Solidus°F | 1598 |
| Densitylb/cu in. at 68°F | 0.301 |
| Specific Gravity | 8.33 |
| Electrical Conductivity% IACS at 68°F | 9 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 18 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10.4 |
| Modulus of Elasticity in Tensionksi | 15000 |
| Poisson's Ratio | 0.32 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Good |
| Seam Weld | Good |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 95 |
| Machinability Rating | 75 |
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod | ASTM | B371/B371M | COPPER-ZINC-SILICON ALLOY ROD | ||
| Rod, Bar & Shapes | Forgings | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES |
Corrosion Properties