Find suppliers for this alloy
C69250
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Not including Ag. |
|||||||||
| Min (%) | 7.5 | 2.0 | 1.0 | 5.0 | |||||
| Max (%) | Rem | 0.05 | 0.20 | 8.5 | 0.20 | 3.0 | 2.0 | 6.0 | 0.10 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| Flat Products & Tubing | 1/2 Hard | H02 |
75 Typ |
| 1/4 Hard | H01 |
65 Typ |
|
| Annealed Tempers, O | O |
58 Typ |
|
| Densitylb/cu in. at 68°F | 0.304 |
|---|---|
| Specific Gravity | 8.41 |
| Electrical Conductivity% IACS at 68°F | 6 |
| Modulus of Elasticity in Tensionksi | 16200 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Excellent |
| Seam Weld | Excellent |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties