Find suppliers for this alloy
C69305
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||||||||||
| Min (%) | 74.0 | 0.15 | 0.05 | 2.5 | ||||||
| Max (%) | 78.0 | 0.09 | 0.30 | Rem | 0.10 | 0.10 | 0.10 | 0.05 | 0.05 | 2.9 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Rod & Bar | 1/2 Hard | H02 |
80 Typ |
41 Typ |
40 Typ |
| Melting Point - Liquidus°F | 1643 |
|---|---|
| Melting Point - Solidus°F | 1607 |
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.3 |
| Electrical Conductivity% IACS at 68°F | 8 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 21.8 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10.3 |
| Modulus of Elasticity in Tensionksi | 15200 |
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties