C69350
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||||||
| Min (%) | 73.0 | .10 | .04 | 3.0 | ||||||
| Max (%) | 77.0 | .20 | .20 | Rem | .50 | .10 | .10 | .10 | .10 | 3.4 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Brinell Hardness, 3000 kg load |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Castings | As Hot Extruded | M30 |
66.7 Min 71.1 Typ 78.3 Max |
15 Min 25 Max |
120 Typ |
| As Hot Forged - Air Cooled | M10 |
66.7 Min 71.1 Typ 78.3 Max |
15 Min 25 Max |
120 Typ |
|
| Melting Point - Solidus°F | 1546 |
|---|---|
| Densitylb/cu in. at 68°F | 0.297 |
| Specific Gravity | 0.297 |
| Electrical Conductivity% IACS at 68°F | 6.5 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 20.13 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.54 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 10.83 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.5 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.095 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Good |
| Seam Weld | Good |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Poor |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 95 |
| Machinability Rating | 75 |
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Marine | Marine Components | ||
| Plumbing | Potable water system components | ||
| Valve Bodies, Faucets and Plumbing Componsnts |
Applicable Specifications
Corrosion Properties