C69450
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu | Pb | Zn | Fe | P | Mn | Si | |
| Min (%) | 80.0 | 0.03 | 3.5 | ||||
| Max (%) | 83.0 | 0.09 | Rem | 0.20 | 0.06 | 0.40 | 4.5 |