Find suppliers for this alloy
C69700
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Mn | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. |
||||||
| Min (%) | 75.0 | 0.50 | 2.5 | |||
| Max (%) | 80.0 | 1.5 | Rem | 0.20 | 0.40 | 3.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Valve Stems | Corrosion Resistance | Corrosion Resistance |
| Valve Stems | Corrosion Resistance | Dezincification Resistance | |
| Valve Stems | Machining Characteristics | Machinability | |
| Valve Stems | Mechanical Properties | HighStrength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod | ASTM | B371/B371M | COPPER-ZINC-SILICON ALLOY ROD |
Corrosion Properties