Find suppliers for this alloy
C69720
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Mn | Sb | Si | |
|
(1) Cu value includes Ag. |
|||||||
| Min (%) | 75.0 | 0.50 | 0.03 | 2.5 | |||
| Max (%) | 80.0 | 1.5 | Rem | 0.20 | 0.40 | 0.06 | 3.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties