C69800
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Ni | Si | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 66.0 | 0.7 | ||||
| Max (%) | 70.0 | 0.8 | Rem | 0.40 | 0.50 | 1.3 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties