Find suppliers for this alloy
C69900
| Elements | ||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Ni | Al | Ag | As | C | Cd | Co | Mn | |
|
(1) Cu value includes Ag. |
||||||||||||
| Min (%) | 1.4 | 40.0 | ||||||||||
| Max (%) | Rem | 0.02 | 0.14 | 0.10 | 0.10 | 2.3 | 0.10 | 0.01 | 0.05 | 0.05 | 0.20 | 48.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties