C70100
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||
| Min (%) | 3.0 | ||||
| Max (%) | Rem | 0.25 | 0.05 | 4.0 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Motor, Rotor Bars | Brazing Characteristics | Brazability |
| Motor, Rotor Bars | Conductivity (Electrical) | Electrical Resistivity |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Condenser & Heat Exchanger Tube with Integral Fins | ASTM | B956/B956M | WELDED COPPER AND COPPER-ALLOY CONDENSER AND HEAT EXCHANGER TUBES WITH INTEGRAL FINS |
Corrosion Properties