Find suppliers for this alloy
C70265
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | P | Ni(3) | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||
| Min (%) | 0.05 | 1.0 | 0.20 | ||||
| Max (%) | Rem | 0.05 | 0.8 | 0.30 | 0.01 | 3.0 | 0.7 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Strip | Mill-hardened Temper, TM - 3/4 HM | TM03 |
105 Min for Standard |
95 Typ |
2 Typ |
| Mill-hardened Temper, TM - 1/2 Hard | TM02 |
90 Min for Standard |
85 Typ |
4 Typ |
|
| Mill-hardened Temper, TM - 1/2 Hard | TM00 |
80 Min for Standard |
65 Typ |
10 Min |
|
| Mill-hardened Temper, TM - 1/2 Hard | TM01 |
90 Min for Standard |
75 Typ |
6 Typ |
|
| Mill-hardened Temper, TM - Hard | TM04 |
110 Min for Standard |
100 Typ |
1 Typ |
|
| Melting Point - Liquidus°F | 1945 |
|---|---|
| Densitylb/cu in. at 68°F | 0.32 |
| Specific Gravity | 8.85 |
| Electrical Conductivity% IACS at 68°F | 40 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 90 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 9 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 9 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 19500 |
| Magnetic Permeability | 1 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Excellent |
| Seam Weld | Excellent |
| Butt Weld | Excellent |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 80 |
Common Fabrication Processes
- Forming and Bending
- Stamping
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors | ||
| Leadframe Sockets |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet & Strip | ASTM | B422/B422M | COPPER-ALUMINUM-SILICON-COBALT ALLOY AND COPPER-NICKEL-ALUMINUM-SILICON ALLOY SHEET AND STRIP | ||
| Strip | ASTM | B888/B88M | COPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS |
Corrosion Properties