Find suppliers for this alloyC70290
Chemical Composition
Element
Cu(1,2)PbSnZnFePNi(3)Si
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co.
Min (%)2.10.021.30.22
Max (%)Rem0.022.70.300.0150.041.70.30
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Flat ProductsMill-hardened Temper, TM - HardTM0485   Typ
75   Typ
15   Min
Mill-hardened Temper, TM - XHMS SpringTM08100   Typ
95   Typ
7   Min
Mill-hardened Temper, TM -XHM - Extra HardTM0695   Typ
85   Typ
10   Min
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1958
Melting Point - Solidus°F1850
Densitylb/cu in. at 68°F0.32
Specific Gravity8.88
Electrical Conductivity% IACS at 68°F30
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F75
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi19000
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingFair
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingFair
Capacity for Being Cold WorkedExcellent
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.