Find suppliers for this alloy
C70370
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni | Ag | Co | Mg | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||||||
| Min (%) | 1.0 | 0.20 | 1.0 | 0.50 | ||||||
| Max (%) | Rem | 0.05 | 1.0 | 0.20 | 2.0 | 0.70 | 2.0 | 0.04 | 0.20 | 1.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Flat Products | Mill-hardened Temper, TM - 1/2 Hard | TM02 |
110 Typ |
100 Typ |
6 Min |
| Mill-hardened Temper, TM - Hard | TM04 |
120 Typ |
110 Typ |
4 Min |
|
| Mill-hardened Temper, TM -XHM - Extra Hard | TM06 |
130 Typ |
120 Typ |
1 Min |
|
| Melting Point - Liquidus°F | 2007 |
|---|---|
| Melting Point - Solidus°F | 1967 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.81 |
| Electrical Conductivity% IACS at 68°F | 50 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.8 |
| Modulus of Elasticity in Tensionksi | 19000 |
| Modulus of Rigidityksi | 7300 |
| Magnetic Permeability | 1.01 |
| Poisson's Ratio | 0.3 |
| Technique | Suitability |
|---|---|
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties