C70700
| Elements | ||||
|---|---|---|---|---|
| Cu(1,2) | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||
| Min (%) | 9.5 | |||
| Max (%) | Rem | 0.05 | 10.5 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Resistance Wire | Conductivity (Electrical) | Electrical Resistivity |
| Resistance Wire | Mechanical Properties | Flexibility |
Applicable Specifications
Corrosion Properties