Find suppliers for this alloy
C71520
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | P | Ni(3) | C | Mn | S | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||||
| Min (%) | 65.0 | 0.40 | 29.0 | ||||||
| Max (%) | 0.02 | 0.50 | 1.0 | 0.02 | 33.0 | 0.05 | 1.0 | 0.02 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Section Size (in) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | As Hot Forged - Air Cooled | M10 |
50 Min |
20 Min |
30 Min |
6 |
| As Hot Forged - Air Cooled | M10 |
45 Min |
18 Min |
30 Min |
||
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Cu-Ni forgings for sea water exposure | Corrosion Resistance | Salt Water Corrosion Resistance |
| Cu-Ni forgings for sea water exposure | Welding Characteristics | Weldability |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Condenser & Heat Exchanger Tube with Integral Fins | ASTM | B956/B956M | WELDED COPPER AND COPPER-ALLOY CONDENSER AND HEAT EXCHANGER TUBES WITH INTEGRAL FINS | ||
| Die | ASTM | B283/B283M | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | ||
| Heat Exchanger Tube | ASTM | B543/B543M | WELDED COPPER AND COPPER ALLOY HEAT EXCHANGER TUBE | ||
| Pipe | ASTM | B466/B466M | SEAMLESS COPPER-NICKEL PIPE AND TUBE | ||
| Welded | ASTM | B608 | WELDED COPPER ALLOY PIPE | ||
| Welded | ASTM | B467 | WELDED COPPER-NICKEL PIPE | ||
| Plate | ASTM | B171/B171M | COPPER ALLOY CONDENSER TUBE PLATES | ||
| Rod | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Rod, Bar & Shapes | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES | ||
| Sheet, Strip, Roller Bar & Plate | ASTM | B122/B122M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL PLATE, SHEET, STRIP, AND ROLLED BAR | ||
| Tube | ASTM | B395/B395M | U-BEND SEAMLESS COPPER AND COPPER ALLOY HEAT EXCHANGER AND CONDENSER TUBES | ||
| Welded | ASTM | B552 | SEAMLESS AND WELDED COPPER-NICKEL TUBES FOR WATER DESALTING PLANTS | ||
| ASTM | B359/B359M | COPPER AND COPPER-ALLOY SEAMLESS CONDENSER AND HEAT EXCHANGER TUBES WITH INTEGRAL FINS | |||
| ASTM | B466/B466M | SEAMLESS COPPER-NICKEL PIPE AND TUBE | |||
| ASTM | B111/B111M | COPPER AND COPPER ALLOY SEAMLESS CONDENSER TUBES AND FERRULE STOCK |
Corrosion Properties