| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2,3) | Pb | Zn | Fe | Ni(4) | C | Mn | |
|
(1) The following additional maximum limits shall apply: Si 0.15% S 0.024% Al 0.05% and P 0.03%. (2) Cu value includes Ag. (3) Cu + Sum of Named Elements 99.5% min. (4) Ni value includes Co. |
|||||||
| Min (%) | 29.0 | ||||||
| Max (%) | Rem | 0.05 | 0.05 | 0.50 | 33.0 | 0.07 | 0.30 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Electronic & Electrical Switch in Corrosive Environment | Conductivity (Electrical) | Electrical Conductivity |
| Electronic & Electrical Switch in Corrosive Environment | Conductivity (Thermal) | Thermal Conductivity | |
| Electronic & Electrical Switch in Corrosive Environment | Corrosion Resistance | Corrosion Resistance | |
| Vacuum Tube | Forming Characteristics | Formability | |
| Vacuum Tube | Welding Characteristics | Weldability | |
| Industrial | Sensor Plates in Corrosive Environment | Conductivity (Electrical) | Electrical Conductivity |
| Sensor Plates in Corrosive Environment | Corrosion Resistance | Corrosion Resistance | |
| Sensor Plates in Corrosive Environment | Corrosion Resistance | Corrosion Resistance to Salt Water |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Plate | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Rod | Welding | AWS | A5.27 | COPPER AND COPPER ALLOY RODS FOR OXYFUEL GAS WELDING | |
| Sheet | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Strip | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS |