C71581
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2,3) | Pb | Fe | Ni(4) | Mn | |
|
(1) Includes P 0.02% max.; Si 0.25% max.; S 0.01% max.; Ti 0.02 - 0.50%. (2) Cu + Sum of Named Elements 99.5% min. (3) Cu value includes Ag. (4) Ni value includes Co. |
|||||
| Min (%) | 0.40 | 29.0 | |||
| Max (%) | Rem | 0.02 | 0.7 | 32.0 | 1.0 |