Find suppliers for this alloy
C71590
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | C | Mn | |
|
(1) The following additional maximum limits shall apply: Si 0.015% S 0.003% Al 0.002% P 0.001% Hg 0.0005% Ti 0.001% Sb 0.001% As 0.001% Bi 0.001% Co 0.05% Mg 0.10% and Oxygen 0.005% Oxygen. For C70690, Co shall be 0.02% max. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||||
| Min (%) | 29.0 | |||||||
| Max (%) | Rem | 0.001 | 0.001 | 0.001 | 0.15 | 31.0 | 0.02 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Plate | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Sheet | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS | ||
| Strip | ASTM | F96 | ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS |
Corrosion Properties