C71600
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Ni(2) | Mn | |
|
(1) Cu value includes Ag. (2) Ni value includes Co. |
||||||
| Min (%) | 4.8 | 29.0 | ||||
| Max (%) | Rem | 0.05 | 1.0 | 5.8 | 33.0 | 1.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties