C71640
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2,3) | Pb(4) | Zn(5) | Fe | Ni(6) | C | Mn | S | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) The following additional maximum limits shall apply: When the product is for subsequent welding applications and is so specified by the purchaser Zn 0.50% P 0.02% Pb 0.02% S 0.02% (0.008% S for C71110) and C 0.05%. (3) Cu value includes Ag. (4) The following additional maximum limits shall apply: When the product is for subsequent welding applications and is so specified by the purchaser Zn 0.50% P 0.02% Pb 0.02% S 0.02% (0.008% S for C71110) and C 0.05%. (5) The following additional maximum limits shall apply: When the product is for subsequent welding applications and is so specified by the purchaser Zn 0.50% P 0.02% Pb 0.02% S 0.02% (0.008% S for C71110) and C 0.05%. (6) Ni value includes Co. |
||||||||
| Min (%) | 1.7 | 29.0 | 1.5 | |||||
| Max (%) | Rem | 0.05 | 1.0 | 2.3 | 32.0 | 0.06 | 2.5 | 0.03 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Tube | ASTM | B552 | SEAMLESS AND WELDED COPPER-NICKEL TUBES FOR WATER DESALTING PLANTS | ||
| Condenser Tube | ASTM | B111/B111M | COPPER AND COPPER ALLOY SEAMLESS CONDENSER TUBES AND FERRULE STOCK | ||
| ASTM | B543/B543M | WELDED COPPER AND COPPER ALLOY HEAT EXCHANGER TUBE |
Corrosion Properties