Find suppliers for this alloy
C71700
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Zn | Fe | Ni(3) | Be | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||
| Min (%) | 0.40 | 29.0 | 0.30 | |||
| Max (%) | Rem | 1.0 | 1.0 | 33.0 | 0.7 | 1.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet, Strip, Roller Bar & Plate | ASTM | B534 | COPPER-COBALT-BERYLLIUM ALLOY, PLATE, SHEET, STRIP, AND ROLLED BAR |
Corrosion Properties