C71900
| Elements | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | P | Ni(3) | C | Cr | Mn | S | Si | Ti | Zr | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||||||||
| Min (%) | 28.0 | 2.2 | 0.20 | 0.01 | 0.02 | ||||||||
| Max (%) | Rem | 0.015 | 0.05 | 0.50 | 0.02 | 33.0 | 0.04 | 3.0 | 1.0 | 0.015 | 0.25 | 0.20 | 0.35 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Fasteners | Fasteners | Corrosion Resistance | Corrosion Resistance |
| Fasteners | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Fasteners | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Fasteners | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Fasteners | Mechanical Properties | Moderate Strength | |
| Fasteners | Softening Resistance | Resistance to Softening | |
| Industrial | Condenser Sheets | Corrosion Resistance | Corrosion Resistance |
| Condenser Sheets | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Condenser Sheets | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Condenser Sheets | Mechanical Properties | Moderate Strength | |
| Condenser Sheets | Softening Resistance | Resistance to Softening | |
| Distillers | Corrosion Resistance | Corrosion Resistance | |
| Distillers | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Distillers | Mechanical Properties | Moderate Strength | |
| Distillers | Softening Resistance | Resistance to Softening | |
| Evaporators | Corrosion Resistance | Corrosion Resistance | |
| Evaporators | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Evaporators | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Evaporators | Mechanical Properties | Moderate Strength | |
| Evaporators | Softening Resistance | Resistance to Softening | |
| Ferrules | Corrosion Resistance | Corrosion Resistance | |
| Ferrules | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Ferrules | Mechanical Properties | Moderate Strength | |
| Ferrules | Softening Resistance | Resistance to Softening | |
| Heat Exchanger Tubes | Corrosion Resistance | Corrosion Resistance | |
| Heat Exchanger Tubes | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Heat Exchanger Tubes | Mechanical Properties | Moderate Strength | |
| Process Equipment | Corrosion Resistance | Corrosion Resistance | |
| Process Equipment | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Process Equipment | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Process Equipment | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Process Equipment | Mechanical Properties | Moderate Strength | |
| Process Equipment | Softening Resistance | Resistance to Softening | |
| Tanks | Corrosion Resistance | Corrosion Resistance | |
| Tanks | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Tanks | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Tanks | Mechanical Properties | Moderate Strength | |
| Tanks | Softening Resistance | Resistance to Softening | |
| Tube Sheets | Corrosion Resistance | Corrosion Resistance | |
| Tube Sheets | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Tube Sheets | Mechanical Properties | Moderate Strength | |
| Tubing | Corrosion Resistance | Corrosion Resistance | |
| Tubing | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Tubing | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Tubing | Mechanical Properties | Moderate Strength | |
| Tubing | Softening Resistance | Resistance to Softening | |
| Valves | Corrosion Resistance | Corrosion Resistance | |
| Valves | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Valves | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Valves | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Valves | Mechanical Properties | Moderate Strength | |
| Valves | Softening Resistance | Resistance to Softening | |
| Vats | Corrosion Resistance | Corrosion Resistance | |
| Vats | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Vats | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Vats | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Vats | Mechanical Properties | Moderate Strength | |
| Vats | Softening Resistance | Resistance to Softening | |
| Vessels | Corrosion Resistance | Corrosion Resistance | |
| Vessels | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Vessels | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Vessels | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Vessels | Mechanical Properties | Moderate Strength | |
| Vessels | Softening Resistance | Resistance to Softening | |
| Water Boxes | Corrosion Resistance | Corrosion Resistance | |
| Water Boxes | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Water Boxes | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Water Boxes | Fouling Resistance | Non-Fouling | |
| Water Boxes | Mechanical Properties | Moderate Strength | |
| Marine | Salt Water Pipe | Corrosion Resistance | Corrosion Resistance |
| Salt Water Pipe | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Salt Water Pipe | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Salt Water Pipe | Fouling Resistance | Non-Fouling | |
| Salt Water Pipe | Mechanical Properties | Moderate Strength | |
| Plumbing | Hot Water Tanks | Corrosion Resistance | Corrosion Resistance |
| Hot Water Tanks | Corrosion Resistance | Corrosion Resistance to 700 F. | |
| Hot Water Tanks | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Hot Water Tanks | Corrosion Resistance | Erosion and Impingement Corrosion Resistance | |
| Hot Water Tanks | Mechanical Properties | Moderate Strength | |
| Hot Water Tanks | Softening Resistance | Resistance to Softening |
Applicable Specifications
Corrosion Properties