Find suppliers for this alloy
C72420
| Elements | ||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Al | C | Cr | Mg | Mn | S | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.7% min. (3) Ni value includes Co. |
||||||||||||||
| Min (%) | 0.7 | 13.5 | 1.0 | 3.5 | ||||||||||
| Max (%) | Rem | 0.02 | 0.10 | 0.20 | 1.2 | 0.01 | 16.5 | 2.0 | 0.05 | 0.50 | 0.05 | 5.5 | 0.15 | 0.15 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties