Find suppliers for this alloy
C72450
| Elements | |||
|---|---|---|---|
| Cu(1) | Ni | Al | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||
| Min (%) | 18.0 | 2.0 | |
| Max (%) | Rem | 25.0 | 4.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| Strip | Ultra Spring | H13 |
188.5 Min 203 Typ 232 Max |
| Densitylb/cu in. at 68°F | .307 |
|---|---|
| Specific Gravity | 8.5 |
| Electrical Conductivity% IACS at 68°F | 8 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 26.5 |
| Modulus of Elasticity in Tensionksi | 21800 |
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties