Find suppliers for this alloy
C72650
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.7% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||
| Min (%) | 4.5 | 7.0 | |||||
| Max (%) | Rem | 0.01 | 5.5 | 0.10 | 0.10 | 8.0 | 0.10 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
YS-0.05% Offset |
Elongation (%) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Strip | 1/2 Hard and Spinodal Hardened (1/2 TS) | TS02 |
135 Min for Standard |
100 Min for Standard |
6 Typ |
|
| 1/4 Hard and Spinodal Hardened (1/4 TS) | TS01 |
130 Min for Standard |
90 Min for Standard |
8 Typ |
||
| 3/4 Hard and Spinodal Hardened (3/4 TS) | TS03 |
140 Min for Standard |
105 Min for Standard |
6 Typ |
||
| Hard and Spinodal Hardened | TS04 |
140 Min for Standard |
110 Min for Standard |
4 Typ |
||
| Mill-hardened Temper, TM - 1/2 Hard | TM02 |
115 Min for Standard |
90 Min for Standard |
85 Min for Standard |
10 Typ |
|
| Mill-hardened Temper, TM - 1/2 Hard | TM00 |
100 Min for Standard |
70 Min for Standard |
65 Min for Standard |
18 Typ |
|
| Mill-hardened Temper, TM - Hard | TM04 |
115 Min for Standard |
100 Min for Standard |
95 Min for Standard |
10 Typ |
|
| Mill-hardened Temper, TM - XHMS Spring | TM08 |
130 Min for Standard |
115 Min for Standard |
105 Min for Standard |
6 Typ |
|
| Mill-hardened Temper, TM -XHM - Extra Hard | TM06 |
120 Min for Standard |
105 Min for Standard |
100 Min for Standard |
10 Typ |
|
| Solution Heat Treated | TB00 |
55 Min for Standard |
21 Min for Standard |
38 Typ |
||
| Solution Heat Treated and Cold Worked: 1/2 Hard | TD02 |
75 Min for Standard |
55 Min for Standard |
5 Typ |
||
| Solution Heat Treated and Cold Worked: 1/4 Hard | TD01 |
60 Min for Standard |
45 Min for Standard |
18 Typ |
||
| Solution Heat Treated and Cold Worked: 3/4 Hard | TD03 |
80 Min for Standard |
68 Min for Standard |
4 Typ |
||
| Solution Heat Treated and Cold Worked: Hard | TD04 |
85 Min for Standard |
77 Min for Standard |
2 Typ |
||
| Spinodal Hardened-Low Strength (ATLS) | TX00 |
120 Min for Standard |
60 Min for Standard |
6 Typ |
||
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors for High Temperatures | Conductivity (Electrical) | Electrical Conductivity |
| Connectors for High Temperatures | Conductivity (Thermal) | Thermal Conductivity | |
| Connectors for High Temperatures | Corrosion Resistance | Corrosion Resistance | |
| Connectors for High Temperatures | Mechanical Properties | High Strength | |
| Connectors for High Temperatures | Softening Resistance | Resistance to Softening | |
| Relays | Conductivity (Electrical) | Electrical Conductivity | |
| Relays | Conductivity (Thermal) | Thermal Conductivity | |
| Relays | Corrosion Resistance | Corrosion Resistance | |
| Relays | Corrosion Resistance | Resistant to Oxidation | |
| Relays | Mechanical Properties | High Modulus of Elasticity | |
| Relays | Mechanical Properties | High Strength | |
| Relays | Softening Resistance | Resistance to Softening | |
| Springs | Conductivity (Electrical) | Electrical Conductivity | |
| Springs | Conductivity (Thermal) | Thermal Conductivity | |
| Springs | Corrosion Resistance | Corrosion Resistance | |
| Springs | Corrosion Resistance | Resistant to Oxidation | |
| Springs | Mechanical Properties | High Modulus of Elasticity | |
| Springs | Mechanical Properties | High Strength | |
| Springs | Softening Resistance | Resistance to Softening | |
| Switches | Conductivity (Electrical) | Electrical Conductivity | |
| Switches | Conductivity (Thermal) | Thermal Conductivity | |
| Switches | Corrosion Resistance | Corrosion Resistance | |
| Switches | Corrosion Resistance | Resistant to Oxidation | |
| Switches | Mechanical Properties | High Modulus of Elasticity | |
| Switches | Mechanical Properties | High Strength | |
| Switches | Softening Resistance | Resistance to Softening | |
| Industrial | Cladding and Inlay | Corrosion Resistance | Corrosion Resistance |
| Cladding and Inlay | Corrosion Resistance | Resistant to Oxidation | |
| Cladding and Inlay | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Strip | ASTM | B740 | STRIPS, COPPER-NICKEL-TIN SPINODAL ALLOY STRIP |
Corrosion Properties