Find suppliers for this alloyC72660
Chemical Composition
Element
Cu(1)PbSnZnFeNi(2)MgMn
(1) Cu + Sum of Named Elements 99.5% min. (2) Includes Co.
Min (%)4.57.0.05
Max (%)Rem.025.5.50.508.0.15.30
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Vickers Hardness, 500 gm
Vickers Hardness, 3000 gm
Rod1/2 Hard and Spinodal Hardened (1/2 TS)TS0266.7   Min
69.6   Typ
72.5   Max
53.7   Min
61.6   Typ
69.6   Max
160   Typ
1/4 Hard and Spinodal Hardened (1/4 TS)TS01105.9   Min
115.3   Typ
124.7   Max
91.4   Min
102.3   Typ
113.01   Max
270   Typ
Precipitation Heat Treated or Spinodal Heat Treated and 1/4 HardTL01113.1   Min
117.5   Typ
121.8   Max
79.8   Min
94.3   Typ
108.8   Max
280   Typ
Precipitation Heat Treated or Spinodal Heat Treated and SpringTL08137.8   Min
148.7   Typ
159.5   Max
132   Min
144.3   Typ
145   Max
330   Typ
Wire1/2 Hard and Spinodal Hardened (1/2 TS)TS0272.5   Min
79.8   Typ
87.0   Max
69.6   Min
74.0   Typ
78.3   Max
200   Typ
1/4 Hard and Spinodal Hardened (1/4 TS)TS0166.7   Min
67.6   Typ
72.5   Max
53.7   Min
61.6   Typ
69.6   Max
3/4 Hard and Spinodal Hardened (3/4 TS)TS0387.0   Min
92.8   Typ
98.6   Max
78.3   Min
83.4   Typ
88.5   Max
220   Typ
Quench HardenedTQ0059.5   Min
63.8   Typ
66.7   Max
53.7   Typ
140   Max
Spinodal Hardened-Low Strength (ATLS) TX00107.3   Typ
95.7   Typ
240   Typ
Spring and Spinodal Hardened TS0898.6   Min
103.0   Typ
107.3   Max
88.5   Min
92.1   Typ
82.1   Typ
240   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Solidus°F1760
Densitylb/cu in. at 68°F0.318
Specific Gravity8.8
Electrical Conductivity% IACS at 68°F13
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F31.7
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingGood
Spot WeldFair
Seam WeldFair
Butt WeldFair
Capacity for Being Cold WorkedExcellent
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConductors
Connector Components
IndustrialScrew Machine Parts, Products
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties