Find suppliers for this alloy
C72950
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.7% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||
| Min (%) | 4.5 | 20.0 | ||||
| Max (%) | Rem | 0.05 | 5.7 | 0.6 | 22.0 | 0.6 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.32 |
|---|---|
| Specific Gravity | 8.86 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties