Find suppliers for this alloy
C73150
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Ni | Mn | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 9.0 | 4.0 | ||||
| Max (%) | Rem | 0.10 | 15.0 | 0.25 | 7.0 | 0.50 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Vickers Hardness, 3000 gm | Section Size (in) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Strip | 1/2 Hard | H02 |
56.7 Min 71.1 Max |
5 Min |
110 Min |
.15 |
| Annealed | O61 |
45.7 Min |
25 Min |
.15 | ||
| Extra Hard | H06 |
76.9 Min 91.4 Max |
150 Min |
.15 | ||
| Hard | H04 |
66.7 Min 81.2 Max |
135 Min |
.15 | ||
| Melting Point - Liquidus°F | 1958 |
|---|---|
| Specific Gravity | 8.77 |
| Electrical Conductivity% IACS at 68°F | 15 |
| Electrical Conductivity% IACS at 68°F | 0.317 |
| Modulus of Elasticity in Tensionksi | 17400 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties