C74300
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||
| Min (%) | 63.0 | 7.0 | ||||
| Max (%) | 66.0 | 0.09 | Rem | 0.25 | 9.0 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Badges, Nameplates | Appearance | Color |
| Badges, Nameplates | Forming Characteristics | Formability | |
| Badges, Nameplates | Plating Characteristics | Plateable | |
| Belt Buckles | Appearance | Color | |
| Belt Buckles | Forming Characteristics | Formability | |
| Belt Buckles | Plating Characteristics | Plateable |
Applicable Specifications
Corrosion Properties