Find suppliers for this alloy
C74400
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.7% min. (3) Ni value includes Co. |
|||||
| Min (%) | 62.0 | 2.0 | |||
| Max (%) | 66.0 | 0.05 | Rem | 0.05 | 4.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm | Section Size (in) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Flat Products | Soft Anneal | O60 |
51 Typ |
17 Typ |
50 Max | 70 Typ |
0.025 |
| Melting Point - Liquidus°F | 1706 |
|---|---|
| Melting Point - Solidus°F | 1670 |
| Densitylb/cu in. at 68°F | 0.308 |
| Specific Gravity | 8.5 |
| Electrical Conductivity% IACS at 68°F | 26 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 67 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15000 |
| Modulus of Rigidityksi | 5600 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Capacity for Being Cold Worked | Excellent |
Common Fabrication Processes
- Blanking
- Roll Forming
- Stamping
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Automotive Radiator Headers | Forming Characteristics | Formability |
| Automotive Radiator Headers | Softening Resistance | Anneal Resistance at Elevated Temperature | |
| Industrial | Heater Headers | Forming Characteristics | Formability |
| Heater Headers | Softening Resistance | Anneal Resistance at Elevated Temperature |
Applicable Specifications
Corrosion Properties