Find suppliers for this alloy
C76400
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||
| Min (%) | 58.5 | 16.5 | ||||
| Max (%) | 61.5 | 0.05 | Rem | 0.25 | 19.5 | 0.50 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.315 |
|---|---|
| Specific Gravity | 8.72 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Holloware | Appearance | Color |
| Holloware | Forming Characteristics | Formability | |
| Holloware | Mechanical Properties | High Strength | |
| Holloware | Plating Characteristics | Plateable | |
| Medallions | Appearance | Color | |
| Medallions | Corrosion Resistance | Corrosion Resistance | |
| Medallions | Forming Characteristics | Coinability | |
| Medallions | Mechanical Properties | High Strength | |
| Plaques | Appearance | Color | |
| Plaques | Corrosion Resistance | Corrosion Resistance | |
| Plaques | Forming Characteristics | Coinability | |
| Plaques | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Rod | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Wire | ASTM | B206/B206M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER WIRE) AND COPPER-NICKEL ALLOY WIRE |
Corrosion Properties