C76800
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||
| Min (%) | 47.5 | 8.0 | 4.5 | ||
| Max (%) | 50.0 | .09 | Rem | 9.5 | 6.5 |
Mechanical Properties
| Melting Point - Liquidus°F | 1686 |
|---|---|
| Melting Point - Solidus°F | 1634 |
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.3 |
| Electrical Conductivity% IACS at 68°F | 4.4 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 14 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 9.4 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 9.4 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.4 |
| Modulus of Elasticity in Tensionksi | 16800 |
| Modulus of Rigidityksi | 6200 |
| Poisson's Ratio | 0.33 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 80 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 1022 | |||
Typical Uses
Applicable Specifications
Corrosion Properties