Find suppliers for this alloy
C77300
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | P | Ni(3) | Al | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||
| Min (%) | 46.0 | 9.0 | 0.04 | ||||
| Max (%) | 50.0 | 0.05 | Rem | 0.25 | 11.0 | 0.01 | 0.25 |
Mechanical Properties
| Melting Point - Liquidus°F | 1715 |
|---|---|
| Melting Point - Solidus°F | 1690 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Excellent |
| Capacity for Being Cold Worked | Fair |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 20 |
Common Fabrication Processes
- Drawing
- Hot Extrusion
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Architecture | Architectural Shapes | Appearance | Color |
| Architectural Shapes | Friction & Wear Properties | Wear Parts | |
| Architectural Shapes | Mechanical Properties | High Strength | |
| Elevators | Appearance | Color | |
| Elevators | Corrosion Resistance | Corrosion Resistance | |
| Elevators | Friction & Wear Properties | Wear Parts | |
| Elevators | Mechanical Properties | High Strength | |
| Handrails | Appearance | Color | |
| Handrails | Friction & Wear Properties | Wear Parts | |
| Thresholds | Appearance | Color | |
| Thresholds | Friction & Wear Properties | Wear Parts | |
| Industrial | Carbide Tips to Saw Blades | Appearance | Silver Color |
| Carbide Tips to Saw Blades | Corrosion Resistance | Corrosion Resistance | |
| Carbide Tips to Saw Blades | Friction & Wear Properties | Bearing Surfaces | |
| Carbide Tips to Saw Blades | Mechanical Properties | Stronger than other Brazing Alloys | |
| Carbide Tips to Snow Plow Blades | Appearance | Silver Color | |
| Carbide Tips to Snow Plow Blades | Corrosion Resistance | Corrosion Resistance | |
| Carbide Tips to Snow Plow Blades | Friction & Wear Properties | Bearing Surfaces | |
| Carbide Tips to Snow Plow Blades | Mechanical Properties | Stronger than other Brazing Alloys | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Appearance | Silver Color | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Conductivity (Electrical) | Electrical Conductivity | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Conductivity (Thermal) | Thermal Conductivity | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Corrosion Resistance | Corrosion Resistance | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Friction & Wear Properties | Bearing Surfaces | |
| Oil Drilling Equip: Welding Rod for Oxyfuel Gas Welding | Mechanical Properties | Stronger than other Brazing Alloys |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Brazing Filler Metal | AWS | A5.8 | BRAZING FILLER METAL |
Corrosion Properties