C77400
| Elements | ||||
|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Ni(3) | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||
| Min (%) | 43.0 | 9.0 | ||
| Max (%) | 47.0 | 0.09 | Rem | 11.0 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.306 |
|---|---|
| Specific Gravity | 8.47 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Architecture | Elevator Trim | Appearance | Color |
| Elevator Trim | Brazing Characteristics | Brazability | |
| Elevator Trim | Corrosion Resistance | Corrosion Resistance | |
| Elevator Trim | Friction & Wear Properties | Wear Resistance | |
| Handrails | Appearance | Appearance | |
| Handrails | Corrosion Resistance | Corrosion Resistance | |
| Handrails | Friction & Wear Properties | Wear Resistance | |
| Thresholds | Appearance | Appearance | |
| Thresholds | Corrosion Resistance | Corrosion Resistance | |
| Thresholds | Friction & Wear Properties | Wear Resistance |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES | ||
| Die | Forgings | ASTM | B283/B283M | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | |
| Rod | Forgings | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES | |
| Shapes | Forgings | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES |
Corrosion Properties