Find suppliers for this alloy
C77600
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||
| Min (%) | 42.0 | 12.0 | |||||
| Max (%) | 45.0 | 0.25 | 0.15 | Rem | 0.20 | 14.0 | 0.25 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Extrusions | As Hot Extruded | M30 |
91 Typ |
47 Typ |
30 Typ |
83 Typ |
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Decorative Molding | ||
| Elevator Sills | |||
| Hardware, Archetectural |
Applicable Specifications
Corrosion Properties