Find suppliers for this alloy
C78600
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Ni | Mn | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 60.0 | 1.25 | 8.5 | |||
| Max (%) | 63.0 | 1.75 | Rem | 0.35 | 11.0 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties