Find suppliers for this alloy
C79000
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||
| Min (%) | 63.0 | 1.5 | 11.0 | |||
| Max (%) | 67.0 | 2.2 | Rem | 0.35 | 13.0 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Key Blanks | Corrosion Resistance | Corrosion Resistance |
| Key Blanks | Machining Characteristics | Machinability | |
| Key Blanks | Mechanical Properties | High Strength |
Applicable Specifications
Corrosion Properties