Find suppliers for this alloy
C79200
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||
| Min (%) | 59.0 | 0.8 | 11.0 | |||
| Max (%) | 66.5 | 1.4 | Rem | 0.25 | 13.0 | 0.50 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.316 |
|---|---|
| Specific Gravity | 8.75 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Builders Hardware | Lock Pins | Corrosion Resistance | Corrosion Resistance |
| Lock Pins | Friction & Wear Properties | Wearability | |
| Lock Pins | Machining Characteristics | Machinability | |
| Lock Pins | Mechanical Properties | High Strength | |
| Consumer | Musical Instrument Parts | Appearance | Color |
| Musical Instrument Parts | Corrosion Resistance | Corrosion Resistance | |
| Musical Instrument Parts | Machining Characteristics | Machinability | |
| Musical Instrument Parts | Mechanical Properties | Moderate Strength | |
| Industrial | Electrodes, Medical EKG and other Medical | Conductivity (Electrical) | Electrical Conductivity |
| Electrodes, Medical EKG and other Medical | Corrosion Resistance | Corrosion Resistance |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Rod | ASTM | B151/B151M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR | ||
| Wire | ASTM | B206/B206M | COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER WIRE) AND COPPER-NICKEL ALLOY WIRE |
Corrosion Properties