| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||
| Min (%) | 59.0 | 0.8 | 23.0 | ||||
| Max (%) | 63.0 | 1.1 | 0.6 | Rem | 0.25 | 26.0 | 0.50 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| Rod | Hard | H04 |
80 Min 87 Typ |
2 Min |
| Hard | H04 |
80 Min 87 Typ |
2 Min |
|
| Hard | H04 |
87 Min 98 Typ |
2 Min |
|
| Wire | Hard | H04 |
80 Min 87 Typ |
2 Min |
| Hard | H04 |
87 Min 98 Typ |
2 Min |
|
| Hard | H04 |
80 Min 87 Typ |
2 Min |
|
| Melting Point - Liquidus°F | 2140 |
|---|---|
| Melting Point - Solidus°F | 2100 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.8 |
| Electrical Conductivity% IACS at 68°F | 4 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 12 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.1 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.095 |
| Modulus of Elasticity in Tensionksi | 24200 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Spot Weld | Not Recommended |
| Seam Weld | Not Recommended |
| Butt Weld | Not Recommended |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Not Recommended |
| Machinability Rating | 60 |
Common Fabrication Processes
- Forming
- Machining
- Stamping
| Treatment | Minimum* | Value* | Time** | |
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 482 | |||
| Solution Treatment | 1382 | 0 | ||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Fasteners | Corrosion Resistance | Corrosion Resistance |
| Fiber Optic Connectors | Magnetic Properties | Non-Magnetic |
Applicable Specifications
Corrosion Properties