Find suppliers for this alloy
C79600
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Includes Co. |
|||||
| Min (%) | 43.5 | 0.8 | 9.0 | 1.5 | |
| Max (%) | 46.5 | 1.2 | Rem | 11.0 | 2.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | Hard | H04 |
70 Typ |
40 Typ |
15 Typ |
70 Typ |
| Melting Point - Liquidus°F | 1700 |
|---|---|
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.39 |
| Electrical Conductivity% IACS at 68°F | 7 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 21 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties