Chemical Composition
Element
Cu(1,2)PbZnNi(3)Mn
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Includes Co.
Min (%)43.50.89.01.5
Max (%)46.51.2Rem11.02.5
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell B scale
RodHardH0470   Typ
40   Typ
15   Typ
70   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1700
Densitylb/cu in. at 68°F0.3
Specific Gravity8.39
Electrical Conductivity% IACS at 68°F7
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F21
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)11
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.