C79620
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Ni | Mn | |
|
(1) Cu value includes Ag. |
|||||
| Min (%) | 46.0 | 0.50 | 8.0 | ||
| Max (%) | 48.0 | 2.0 | Rem | 11.0 | 0.50 |