| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||
| Min (%) | 45.5 | 1.5 | 9.0 | 1.5 | ||
| Max (%) | 48.5 | 2.5 | Rem | 0.25 | 11.0 | 2.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Musical Instrument Parts | Appearance | Color |
| Musical Instrument Parts | Machining Characteristics | Machinability | |
| Musical Instrument Parts | Mechanical Properties | High Strength |
Applicable Specifications
Corrosion Properties