Find suppliers for this alloy
C80100
| Elements | |
|---|---|
| Cu(1) | |
|
(1) Cu value includes Ag. |
|
| Min (%) | 99.95 |
| Max (%) | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Fatigue Strength** (ksi) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | |||||||
| As Sand Cast | As Sand Cast | M01 |
25 Typ |
9 Typ |
40 Typ |
44 Typ |
9 Typ |
| Melting Point - Liquidus°F | 1981 |
|---|---|
| Melting Point - Solidus°F | 1948 |
| Densitylb/cu in. at 68°F | 0.323 |
| Specific Gravity | 8.94 |
| Electrical Conductivity% IACS at 68°F | 100 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 226 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.4 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.092 |
| Modulus of Elasticity in Tensionksi | 17000 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Not Recommended |
| Machinability Rating | 10 |
Common Fabrication Processes
| Treatment | Time** | |||
|---|---|---|---|---|
| ** Time is measured in minutes. | ||||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Weld Guns | Conductivity (Thermal) | Thermal Conductivity |
| Weld Guns | Corrosion Resistance | Corrosion Resistance | |
| Weld Guns | Corrosion Resistance | Oxidation Resistance | |
| Electrical | Bus Conductors | Conductivity (Electrical) | Electrical Conductivity |
| Bus Conductors | Corrosion Resistance | Corrosion Resistance | |
| Bus Conductors | Corrosion Resistance | Oxidation Resistance | |
| Connectors | Conductivity (Electrical) | Electrical Conductivity | |
| Connectors | Conductivity (Thermal) | Thermal Conductivity | |
| Connectors | Corrosion Resistance | Corrosion Resistance | |
| Connectors | Corrosion Resistance | Oxidation Resistance | |
| Hollow Conductors | Conductivity (Electrical) | Electrical Conductivity | |
| Hollow Conductors | Conductivity (Thermal) | Thermal Conductivity | |
| Hollow Conductors | Corrosion Resistance | Corrosion Resistance | |
| Hollow Conductors | Corrosion Resistance | Oxidation Resistance | |
| Industrial | Electrode Holders | Conductivity (Electrical) | Electrical Conductivity |
| Electrode Holders | Conductivity (Thermal) | Thermal Conductivity | |
| Electrode Holders | Corrosion Resistance | Corrosion Resistance | |
| Electrode Holders | Corrosion Resistance | Oxidation Resistance | |
| Electrode Plates For Process Industry Machinery | Conductivity (Electrical) | Electrical Conductivity | |
| Electrode Plates For Process Industry Machinery | Conductivity (Thermal) | Thermal Conductivity | |
| Electrode Plates For Process Industry Machinery | Corrosion Resistance | Corrosion Resistance | |
| Electrode Plates For Process Industry Machinery | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
| Electrode Plates For Process Industry Machinery | Corrosion Resistance | Oxidation Resistance | |
| Rings for Process Industry Machinery | Conductivity (Electrical) | Electrical Conductivity | |
| Rings for Process Industry Machinery | Conductivity (Thermal) | Thermal Conductivity | |
| Rings for Process Industry Machinery | Corrosion Resistance | Corrosion Resistance | |
| Rings for Process Industry Machinery | Corrosion Resistance | Oxidation Resistance |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Ingot | FEDERAL | QQ-C-521 | COPPER INGOT |
Corrosion Properties