Find suppliers for this alloyC80100
Chemical Composition
Element
Cu(1)
(1) Cu value includes Ag.
Min (%)99.95
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
Fatigue Strength**
(ksi)
As Sand CastAs Sand CastM0125   Typ
9   Typ
40   Typ
44   Typ
9   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
Melting Point - Liquidus°F1981
Melting Point - Solidus°F1948
Densitylb/cu in. at 68°F0.323
Specific Gravity8.94
Electrical Conductivity% IACS at 68°F100
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F226
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.4
Specific Heat CapacityBtu/ lb /°F at 68°F0.092
Modulus of Elasticity in Tensionksi17000
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingFair
Coated Metal Arc WeldingNot Recommended
Machinability Rating10
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
AutomotiveWeld GunsConductivity (Thermal)Thermal Conductivity
Weld GunsCorrosion ResistanceCorrosion Resistance
Weld GunsCorrosion ResistanceOxidation Resistance
ElectricalBus ConductorsConductivity (Electrical)Electrical Conductivity
Bus ConductorsCorrosion ResistanceCorrosion Resistance
Bus ConductorsCorrosion ResistanceOxidation Resistance
ConnectorsConductivity (Electrical)Electrical Conductivity
ConnectorsConductivity (Thermal)Thermal Conductivity
ConnectorsCorrosion ResistanceCorrosion Resistance
ConnectorsCorrosion ResistanceOxidation Resistance
Hollow ConductorsConductivity (Electrical)Electrical Conductivity
Hollow ConductorsConductivity (Thermal)Thermal Conductivity
Hollow ConductorsCorrosion ResistanceCorrosion Resistance
Hollow ConductorsCorrosion ResistanceOxidation Resistance
IndustrialElectrode HoldersConductivity (Electrical)Electrical Conductivity
Electrode HoldersConductivity (Thermal)Thermal Conductivity
Electrode HoldersCorrosion ResistanceCorrosion Resistance
Electrode HoldersCorrosion ResistanceOxidation Resistance
Electrode Plates For Process Industry MachineryConductivity (Electrical)Electrical Conductivity
Electrode Plates For Process Industry MachineryConductivity (Thermal)Thermal Conductivity
Electrode Plates For Process Industry MachineryCorrosion ResistanceCorrosion Resistance
Electrode Plates For Process Industry MachineryCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Electrode Plates For Process Industry MachineryCorrosion ResistanceOxidation Resistance
Rings for Process Industry MachineryConductivity (Electrical)Electrical Conductivity
Rings for Process Industry MachineryConductivity (Thermal)Thermal Conductivity
Rings for Process Industry MachineryCorrosion ResistanceCorrosion Resistance
Rings for Process Industry MachineryCorrosion ResistanceOxidation Resistance
Applicable Specifications
Form System Standard Description
IngotFEDERALQQ-C-521COPPER INGOT
Corrosion Properties

No information available.