Chemical Composition
Elements
Cu(1)
(1) Cu value includes Ag.
Min (%) 99.9
Max (%)
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell F scale
* Measured at room temperature, 68°F (20°C).
As Centrifugal Cast As Centrifugal Cast M02 20 Min
25 Typ
6.5 Min
8 Typ
20 Min
25 Typ
30 Typ
Physical Properties
Melting Point - Liquidus°F 1981
Melting Point - Solidus°F 1948
Densitylb/cu in. at 68°F 0.323
Specific Gravity 8.94
Electrical Conductivity% IACS at 68°F 98
Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) 9.4
Modulus of Elasticity in Tensionksi 17000
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical uses
Product Category Product Reason Category Reason
Electrical Electrical Conductors Conductivity (Electrical) Electrical Conductivity
Electrical Conductors Conductivity (Thermal) Thermal Conductivity
Electrical Conductors Corrosion Resistance Corrosion Resistance
Electrical Conductors Corrosion Resistance Oxidation Resistance
Industrial Corrosion and Oxidation Resistant Applications Conductivity (Electrical) Electrical Conductivity
Corrosion and Oxidation Resistant Applications Conductivity (Thermal) Thermal Conductivity
Corrosion and Oxidation Resistant Applications Corrosion Resistance Corrosion Resistance
Corrosion and Oxidation Resistant Applications Corrosion Resistance Oxidation Resistance
Rotor End Rings Conductivity (Electrical) Electrical Conductivity
Rotor End Rings Conductivity (Thermal) Thermal Conductivity
Rotor End Rings Corrosion Resistance Corrosion Resistance
Rotor End Rings Corrosion Resistance Oxidation Resistance
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No Corrosion Properties Available.